    In the modern blast furnaces, the charge consists of a mixture of

    A) Calcined iron oxides + lime + anthracite coal

    B) Calcined iron oxides + limestone + coke

    C) Hydrated iron oxides + dolomite + coke

    D) Iron pyrites + lime +bituminous coal

    Correct Answer: B