    In order to refine "Blister copper" it is melted in a furnace and is stirred with green logs of wood. The purpose is

    A)  To expel the dissolved gases in blister copper

    B)  To bring the impurities to surface and oxidize them

    C)  To increase the carbon content of copper

    D)  To reduce the metallic oxide impurities with hydrocarbon gases liberated from the wood

    Correct Answer: D

    Solution :

    Blister copper contain \[98%\] \[Cu\]and \[2%\]impurities. Blister \[Cu\] is heated in the presence of air in a reverberatory furnace. Molten metal is now stirred with green wood poles. The hydrocarbons liberated from green wood poles reduce \[C{{u}_{2}}O\] into \[Cu\]. Copper thus obtained is \[99.5%\] pure.